Hastelloy
Aloi ya Joto la Juu
◆Hastelloy B ni aloi inayostahimili kutu yenye nguvu ya kupunguza kutu, inafaa kwa asidi ya sulfuriki iliyokolea iliyokolea na vifaa vya gesi ya kloridi hidrojeni na vijenzi.
◆Hastelloy B-2 ina muundo wa fuwele wa ujazo unaozingatia uso.Kwa kudhibiti maudhui ya chuma na chromiamu kwa kiwango cha chini zaidi, inapunguza wepesi wa uchakataji na kuzuia kunyesha kwa awamu ya Ni4Mo kati ya 700-870°C.Inatumika sana katika kemia, petrochemical, utengenezaji wa nishati na uwanja wa udhibiti wa uchafuzi wa mazingira.
◆Hastelloy B-3 ina ukinzani bora wa kutu kwa halijoto yoyote na mkusanyiko wa asidi hidrokloriki.
◆Hastelloy C ina ukakamavu mzuri na ukinzani wa kutu kwa 650-1040℃.
◆Hastelloy C-4 ni aloi inayostahimili ulikaji kiwanja cha redoksi iliyo na ioni za kloridi, na ina uthabiti mzuri wa mafuta.Inatumika katika vifaa vya kloridi ya klorini mvua, asidi ya hypochlorous, asidi ya sulfuriki, asidi hidrokloriki, na asidi mchanganyiko.Inatumika moja kwa moja baada ya kulehemu.
◆Hastelloy C-22 ni aloi yenye maudhui ya juu ya molybdenum, tungsten na chromium, ambayo hutumiwa sana katika nyanja za kemikali na petrokemikali, na uhandisi wa michakato mbalimbali ya kemikali yenye sifa za oxidation na kupunguza.
◆Hastelloy C-276 ina upinzani bora wa shimo, upinzani wa kutu sare, upinzani wa kutu kati ya punjepunje na sifa nzuri za mitambo ya hali ya juu ya joto.Inatumika sana katika tasnia ya nyuklia, kemikali, mafuta ya petroli na tasnia ya madini isiyo na feri.
◆Hastelloy C-2000 ni aloi ya kina zaidi inayostahimili kutu, ambayo ina upinzani bora dhidi ya kutu sare katika mazingira ya vioksidishaji na ya kupunguza.
◆HastelloyG-3 ina upinzani bora kutu na uthabiti wa joto, na ina utendakazi bora katika asidi ya fosforasi na vioksidishaji vingine vikali vya asidi mchanganyiko.
◆HastelloyX ina upinzani wa juu wa kutu na inafaa kwa tasnia mbalimbali za mashine katika mazingira yenye asidi.
Muundo wa kemikali
Daraja | C | P | S | Mn | Si | Ni | Cr | Co | Cu | Fe | N | Mo | Al | W | V | Ti | nyingine |
hakuna kubwa kuliko | |||||||||||||||||
HastelloyB | 0.05 | 0.04 | 0.03 | 1 | 1 | msingi | ≤1 | ≤2.5 | - | 4~6 | - | 26-30 | - | - | 0.2 ~ 0.4 | - | - |
HastelloyB-2 | 0.02 | 0.04 | 0.03 | 1 | 0.1 | msingi | ≤1 | ≤1 | - | ≤2 | - | 26-30 | - | - | - | - | |
HastelloyB-3 | 0.01 | 0.04 | 0.03 | 3 | 0.1 | ≥65 | 1~3 | ≤3 | ≤0.2 | 1~3 | - | 27-32 | ≤0.5 | ≤3 | ≤0.2 | ≤0.2 | - |
HastelloyC | 0.08 | 0.04 | 0.03 | 1 | 1 | msingi | 14.5-16.5 | ≤2.5 | - | 4~7 | - | 15-17 | - | 3 -4.5 | ≤0.35 | - | - |
HastelloyC-4 | 0.015 | 0.04 | 0.03 | 1 | 0.08 | msingi | 14-18 | ≤2 | - | ≤3 | - | 14-17 | - | - | - | ≤0.7 | - |
HastelloyC-22 | 0.015 | 0.025 | 0.01 | 0.5 | 0.08 | msingi | 20 -22.5 | ≤2.5 | - | 2 - 6 | - | 12.5-14.5 | - | 2.5-3.5 | ≤0.35 | - | - |
HastelloyC-276 | 0.01 | 0.04 | 0.03 | 1 | 0.08 | msingi | 14.5-16.5 | ≤2.5 | - | 4~7 | - | 15-17 | - | 3 -4.5 | ≤0.35 | - | - |
HastelloyC-2000 | 0.01 | 0.025 | 0.01 | 0.5 | 0.08 | msingi | 22-24 | ≤2 | 1.3-1.9 | 3 | - | 15-17 | ≤0.5 | - | - | - | - |
HastelloyG-3 | 0.015 | 0.03 | 0.03 | 1 | 1 | msingi | 21-23.5 | ≤5 | 1.5-2.5 | 18-21 | - | 6-8 | - | ≤1.5 | - | - | Nb/Ta0.3~1.5 |
HastelloyX | 0.1 | 0.025 | 0.015 | 1 | 1 | msingi | 20.5-23 | 0.5 ~ 2.5 | - | 17-20 | - | 8~10 | ≤0.5 | 0.2~1 | - | ≤0.15 | - |
Kiwango cha chini cha mali ya Aloi
Daraja | jimbo | nguvu ya mkazo RmN/m㎡ | Nguvu ya Mazao Rp0.2N/m㎡ | Elongation As% | Ugumu wa Brinell HB |
HastelloyB | suluhisho thabiti | 690 | 310 | 40 | - |
HastelloyB-2 | suluhisho thabiti | 690 | 310 | 40 | - |
HastelloyB-3 | suluhisho thabiti | 690 | 290 | 42 | - |
HastelloyC | suluhisho thabiti | 690 | 300 | 41 | - |
HastelloyC-4 | suluhisho thabiti | 650 | 280 | 40 | - |
HastelloyC-22 | suluhisho thabiti | 690 | 283 | 40 | - |
HastelloyC-276 | suluhisho thabiti | 690 | 283 | 40 | - |
HastelloyC-2000 | suluhisho thabiti | 700 | 290 | 40 | - |
HastelloyG-3 | suluhisho thabiti | 700 | 300 | 40 | - |
HastelloyX | suluhisho thabiti | 725 | 310 | 30 | - |