KARATASI ZA DATA YA ALOY 625
Muundo wa Kemikali
Muundo wa Kemikali | Cr | Ni | Mo | Co | Cb+Ta | Al | Ti | C | Fe | Me | Mn | Si | P | S |
% Thamani (kiwango cha chini) | 20.0 |
| 8.0 | - | 3.15 | - | - | - | - |
| - | - | - | - |
% Thamani (kiwango cha juu) | 23.0 | bal | 10.0 | 1.0 | 4.15 | 0.4 | 0.4 | 0.1 | 5.0 |
| 0.5 | 0.5 | 0.015 | 0.015 |
Sifa za Mitambo
Sifa za Mitambo na Kimwili | 21°C | 204°C | 316°C | 427°C | 538°C | 649°C | 760°C | 871°C |
Ultimate Tensile Strength /Mpa | 992.9 | 923.9 | 910.1 | 910.1 | 896.3 | 820.5 | 527.8 | 275.8 |
0.2% Nguvu ya Mazao /MPa | 579.2 | 455.1 | 434.4 | 420.6 | 420.6 | 413.7 | 406.8 | 268.9 |
Elongation % | 44 | 45 | 42.5 | 45 | 48 | 34 | 59 | 117 |
Mgawo wa Upanuzi wa Joto um/moC | - | 13.1 | 13.3 | 13.7 | 14 | 14.8 | 15.3 | 15.8 |
Uendeshaji wa mafuta /kcal/(hr.mc) | 8.5 | 10.7 | 12.2 | 13.5 | 15 | 16.4 | 17.9 | 19.6 |
Modulus ya Elasticity/ MPa | 2.07 | 1.93 | 1.93 | 1.86 | 1.79 | 1.65 | 1.59 | - |
Maombi
● Mifumo ya kutolea nje ya injini ya ndege
● Mifumo ya kirudisha nyuma ya injini
● Mifumo ya mifereji ya ndege
● Pete za sanda za turbine
● Mivumo na viungo vya upanuzi
● Vipengele vya maji ya bahari
● Vifaa vya mchakato wa kemikali
Upinzani wa kutu
Aloi 625 imestahimili mazingira mengi ya kutu.Katika alkali, maji ya chumvi, maji safi, chumvi za neutral, na katika hewa, karibu hakuna mashambulizi hutokea.Nikeli na chromium hutoa upinzani kwa mazingira ya vioksidishaji.Nickel na molybdenum hutoa upinzani dhidi ya hali ya hewa isiyo na vioksidishaji.
Kutua kwa shimo na nyufa huzuiwa na molybdenum.Niobium huimarisha aloi dhidi ya uhamasishaji wakati wa kulehemu.Upinzani wa kupasuka kwa mkazo wa kloridi ni bora.Aloi hupinga kuongeza na oxidation kwenye joto la juu.
Malipo
PRODUCT FORM | UKUBWA KUTOKA | UKUBWA WA SIZE HADI |
Aloi 625 bomba | inchi 0.5 | 8 ndani |
Aloi 625 coil | 0.25 mm | 3.18 mm |
Aloi 625 waya ya kulehemu | 0.5 mm | 3.175 mm |
Aloi 625 karatasi & sahani | 0.25 mm | 76.2 mm |
Aloi 625 bar pande zote | 12 mm | 260 mm |
Aloi 625 mabomba fittings | inchi 0.5 | 8 ndani |
Aloi 625 filanges | inchi 0.5 | 8 ndani |