HASTELLOY B2 UNS N10665 W.NR.2.4617
Muundo wa Kemikali
Aloi | kipengele | C | Si | Mn | S | P | Ni | Cr | Mo | Fe | Co |
Aloi B2 | Dak | 26.0 | |||||||||
Max | 0.02 | 0.10 | 1.00 | 0.03 | 0.04 | Mizani | 1.0 | 30.0 | 2.0 | 1.0 |
Sifa za Mitambo
Hali ya Aolly | Nguvu ya mkazo Rm Mpa Dak | Nguvu ya mavuno RP 0. 2 Mpa Dak | Kurefusha A 5% Dak |
Suluhisho | 745 | 325 | 40 |
Sifa za Kimwili
Uzito g/cm3 | Kiwango Myeyuko ℃ |
9.2 | 1330~1380 |
Kawaida
Fimbo, Baa, Waya na Hisa za Kughushi- ASTM B 335(Rod, Bar), ASTM B 564(Forging),ASTM B 366(Inayofaa)
Bamba, Karatasi na Ukanda- ASTM B 333
Bomba na bomba- ASTM B 622(Imefumwa ) ASTM B 619/B626(Tube Iliyounganishwa)
Tabia ya Hastelloy B2
● Ustahimilivu mkubwa dhidi ya kupasuka kwa kutu na dhiki
● Ustahimilivu mkubwa katika kupunguza hali kama vile kloridi hidrojeni, salfa, asetiki na asidi fosforiki.
● Ustahimilivu wa asidi hidrokloriki katika viwango na halijoto zote
● Iliyotangulia: Aloi ya INCONEL® C-276 UNS N10276/W.Nr. 2.4819
● Inayofuata: HASTELLOY B-3 UNS N10675/W.Nr.2.4600
Kwa nini Utuchague:
1. Timu ya kitaalamu ya R&D
Usaidizi wa majaribio ya programu huhakikisha kwamba huna wasiwasi tena kuhusu zana nyingi za majaribio.
2. Ushirikiano wa uuzaji wa bidhaa
Bidhaa hizo zinauzwa kwa nchi nyingi duniani kote.
3. Udhibiti mkali wa ubora
4. Wakati wa utoaji imara na udhibiti wa wakati wa utoaji wa utaratibu unaofaa.
Sisi ni timu ya kitaaluma, wanachama wetu wana uzoefu wa miaka mingi katika biashara ya kimataifa. Sisi ni timu changa, iliyojaa msukumo na uvumbuzi. Sisi ni timu ya kujitolea. Tunatumia bidhaa zilizohitimu kuridhisha wateja na kupata imani yao. Sisi ni timu yenye ndoto. Ndoto yetu ya kawaida ni kuwapa wateja bidhaa za kuaminika zaidi na kuboresha pamoja. Tuamini, kushinda-kushinda.