Hastelloy B
Muundo wa Kemikali
Aloi | kipengele | C | Si | Mn | S | P | Ni | Cr | Mo | Fe | Co |
Aloi B2 | Dak | 26.0 | |||||||||
Max | 0.02 | 0.10 | 1.00 | 0.03 | 0.04 | Mizani | 1.0 | 30.0 | 2.0 | 1.0 |
Sifa za Mitambo
Hali ya Aolly | Nguvu ya mkazo Rm Mpa Dak | Nguvu ya mavuno RP 0. 2 Mpa Dak | Kurefusha A 5% Dak |
Suluhisho | 745 | 325 | 40 |
Sifa za Kimwili
Uzito g/cm3 | Kiwango Myeyuko ℃ |
9.2 | 1330~1380 |
Kawaida
Fimbo, Baa, Waya na Hisa za Kughushi- ASTM B 335(Rod, Bar), ASTM B 564(Forging),ASTM B 366(Inayofaa)
Bamba, Karatasi na Ukanda- ASTM B 333
Bomba na bomba- ASTM B 622(Imefumwa ) ASTM B 619/B626(Tube Iliyounganishwa)
Tabia ya Hastelloy B2
● Ustahimilivu mkubwa dhidi ya kupasuka kwa kutu na dhiki
● Ustahimilivu mkubwa katika kupunguza hali kama vile kloridi hidrojeni, salfa, asetiki na asidi fosforiki.
● Ustahimilivu wa asidi hidrokloriki katika viwango na halijoto zote
● Iliyotangulia: Aloi ya INCONEL® C-276 UNS N10276/W.Nr. 2.4819
● Inayofuata: HASTELLOY B-3 UNS N10675/W.Nr.2.4600
Timu yetu sio tu kikundi cha wataalamu walio na uzoefu wa miaka mingi katika biashara ya kimataifa. Sisi ni wabunifu, tunatafuta kila mara kusukuma mipaka ya kile kinachowezekana. Utumiaji wetu wa bidhaa za kisasa kama vile Hastelloy B2 UNS N10665 W.NR.2.4617 unaonyesha dhamira yetu ya kukaa mbele ya shindano na kutoa huduma bora zaidi kwa wateja wetu. Jiunge nasi kwenye azma yetu ya kuleta matokeo ya kudumu katika tasnia na ujionee mwenyewe uwezo wa fikra bunifu.